Design and verification of pressure curve for anti-gravity casting of nickel-base superalloy https://jam.biam.ac.cn/EN/10.11868/j.issn.1005-5053.2021.000190
请登录并选择要私信的好友
300
Design and verification of pressure curve for anti-gravity casting of nickel-base superalloy https://jam.biam.ac.cn/EN/10.11868/j.issn.1005-5053.2021.000190